On faceting instability of Pt (110) under catalytic oxidation of adsorbed CO

M. Papoular

Centre National de la Recherche Scientifique, Centre de Recherches sur les Très Basses Températures, B.P. 166, 38042 Grenoble Cedex 9, France

(Received 17 February 1992, accepted 25 March 1992)

Abstract
The microfaceting, under catalytic oxidation of carbon monoxide, of the (110) surface of platinum is discussed from the point of view that Pt mass transport, as involved in the process, should be energetically assisted by the reaction itself. We give an evaluation of the relative contributions to the relevant surface energy, and of the time required to complete the morphological transformation.

Résumé
La face (110) du platine, soumise à l'oxydation catalytique CO $+\frac{1}{2}$O $_2\to$CO 2, se déforme en microfacettes sous certaines conditions de pression et de température [1-4]. Nous suggérons que cette transformation est assistée mécaniquement par la réaction elle-même. On donne une évaluation des différentes contributions à l'énergie de surface et du temps caractéristique de la transformation morphologique.